# What Causes Pinholes in Pottery and How to Prevent Them

Learn what causes pinholes in pottery glaze, how trapped gas and firing affect the surface, and practical steps to prevent these small glaze defects.

Pinholes in pottery are small holes left in the glaze surface when gas escapes during firing and the glaze does not heal over the opening. The cause sits somewhere in the clay body, the glaze, or the kiln schedule, and fixing it means finding which of those released the gas. This page explains each cause and the steps that keep the fired surface whole. 

## Trapped gas from the clay body 

Pinholes appear when gas trapped inside the clay body pushes out through the melting glaze. Organic matter, carbonates, and moisture in the clay turn to gas as the kiln heats, and a thick or underfired bisque can seal those gases in. A bisque firing that is slow enough and hot enough lets the clay body release its gases before the glaze begins to melt. Holding the kiln near the top of the bisque range gives those gases time to leave. 

## Glaze bubbles that fail to heal 

Bubbles in glaze can burst at peak temperature and leave a pinhole if the glaze is too viscous to flow back. Overfiring makes a glaze thin and runny, while underfiring leaves it stiff and unable to smooth a burst bubble. Very thick glaze application adds another layer that traps gas below the surface. Testing a glaze on a small tile shows how it flows before you commit a whole piece. 

## Kiln firing and cooling choices 

The kiln firing schedule controls when gas leaves and whether the glaze has time to close over it. A soak at peak temperature lets bubbles rise and break while the glaze is still fluid enough to heal. Fast cooling can freeze a burst bubble in place before the surface smooths. Slowing the climb through the temperature range where the clay body outgasses also reduces gas that reaches the glaze. 

## Questions About Pinholes in Pottery 

### What causes pinholes in pottery? 

Pinholes in pottery come from gas that escapes through the glaze during firing and leaves a small opening behind. The gas can originate in the clay body, in the glaze itself, or from moisture and organic material burning out. When the glaze is too stiff or the firing too fast, that opening does not close over. 

### How do I stop pinholes from forming? 

You prevent pinholes by giving gas a clear path out before the glaze seals the surface. Fire the bisque slowly and high enough to burn out carbon and moisture, and apply the glaze in even coats rather than heavy layers. Add a soak at peak temperature so bubbles can rise and the glaze can heal. 

### Does bisque firing affect pinholes? 

Yes, bisque firing affects pinholes because it is the stage where the clay body releases most of its gas. An underfired or fast bisque leaves carbon and moisture in the clay, and those turn to gas later under the glaze. A slower bisque with a hold near the top of the range reduces that risk. 

### Can I fix pinholes after firing? 

Pinholes can sometimes be improved after firing, but the surface will not match an undamaged glaze. Refiring the piece to a temperature where the glaze softens may let it flow and close small holes. Deep or numerous pinholes on a food surface are better treated as a fault, because the openings can harbor residue.